NASH880 is an austenitic stainless steel which was developed by Nippon Yakin. It is suitable for use in high-grade sheathed heater tubes and provides excellent corrosion resistance in wet environments such as hot water supply devices. Nippon Yakin supplies NASH880 in sheet and strip forms.

Chemical Composition 25Ni-23.5Cr-1.2Mo-0.3Al-0.3Ti
Product Shape Coil Sheet
Weldability NAS H880 welded tube has good formability. There is no crack on the bead after several forming tests.
Blackening Property Emissivity of NAS H880 after blackening heat treatment is the same level as alloy 800 (Low C%).
Heat Treatment Heat treatment of NASH880 can be performed in the same manner as with other austenitic stainless steels. The heat treatment temperature range which is normally used is as follows:
Solution treatment: 1000~1100℃; water cooling
Applications Sheathed heater, Furnace parts

Steel Grade/Standard

Nippon Yakin Grade JIS ASTM EN
NASH880

Chemical Composition

Specification C Si Mn P S Ni Cr Mo Cu Al Ti Co N
NASH880 ≤0.030 0.30 – 0.50 0.35 – 0.65 ≤0.025 ≤0.002 24.50 – 27.00 22.80 – 23.90 1.15 – 1.35 ≤0.25 0.20 – 0.40 0.25 – 0.45 0.05 – 1.00 ≤0.02

Physical Properties

Density [g/cm³] 7.92
Specific heat [J/kg·K] 462
Electrical resistivity [µΩ·cm] 92.5
Thermal conductivity [W/m·K] 12.3
Average coefficient of thermal expansion [10⁻⁶/°C] 25 – 200°C: 15.6
25 – 400°C: 16.4
25 – 600°C: 16.8
25 – 800°C: 17.6
25 – 1,000°C: 18.4
Young’s modulus [MPa] 19.4 × 10⁴
Magnetism None
Melting range [°C] 1,380 – 1,407

Mechanical Properties

Mechanical Properties at Room Temperature

Specification 0.2% proof stress [MPa] Tensile strength [MPa] Elongation [%]
Specification (NASH880) ≥205 ≥520 ≥30
Example: Cold-rolled sheet 0.5mm 280 587 42

High Temperature Strength

Corrosion Resistance

1. Crevice Corrosion Resistance

Test condition
① Multicrevice test piece
② Test temperature: 80°C
③ Test time: 24 hr

NaCl 5% 10%
alloy825 NASH880 alloy825 NASH880
alloy825 ×
alloy 800 (Low C%) × ×

○: No corrosion      ×: Corrosion

2. Stress Corrosion Cracking Resistance

Test condition
① U-bend test piece
② Liquid solution: 10% NaCl
③ Test time: 74 hr

Temperature 180°C 200°C 220°C
alloy825 NASH880 alloy825 NASH880 alloy825 NASH880
alloy825 × ×
alloy 800 (Low C%)

○: No SCC      ×: SCC

Weldability

NASH880 welded tube has good formability.
There is no crack on the head after several forming tests.

Flaring test

Flattening test 180° Bending test (R=14mm)

Formability of NASH880 welded tubes (8mmφ × 0.5mmt)

Blackening Property

Emissivity of NASH880 after blackening heat treatment is the same level as alloy 800 (Low C%).

NASH880

NASH880

Alloy 800 (Low C%)

Appearance after blackening test

Heat Treatment

Heat treatment of NASH880 can be performed in the same manner as with other austenitic stainless steels. The heat treatment temperature range which is normally used is as follows:
Solution treatment: 1,000–1,100°C; water cooling

REQUEST QUOTATION

PAYMENT

payment-methods

 

TOOLS & EQUIPMENT

Lifting
Eagle Clamp | Eagle Jack | Elephant | Endo Kogyo
Japan Clamp | Kanetec | Jung | KITO | Katsuyama Kikai
Kondotec | Miki Netsuren | Sanei Seiki | Taiyo

Hand Tools
Bix | Miyakawa | Nakatani Kikai | Ogura | Osakada Tool
Super Tool | TONE | Yutani

Tape
Kamoi | Kikusui | Misuzu | Nirei | Okamoto | Taiho | Teraoka

Measurement
Hasegawa | Kawaki | Kett | KGK | Line Seiki | Nagano Keiki
Niigata Seiki | Obishi Keiki | RSK | Ryoden Shonan | Sanko
Sanwa Supply | Showa Seisakusho | Showa Sokki
SK Sato | Tokyo Keiso | Tokyo Sokushin

Safety Tools
Fujii Denko | Shigematsu | Titan

Welding
Asahi Weldex | Daihen | Koike | Nissan Tanaka

Drilling
Dijet | Kansai Kogu | Nitto Kohki | Okazaki Seiko | Takeda

Chemical
Cemedine | DaitoNippon Grease | Taseto

Other Tools
Hammer Caster | Kitagawa | Matsuda Seiki | Misuz | Sanritsu
Sanyutec | Shizuoka Seiki | Toyo Kensetsu Kohki | Yamamoto
Yamari

PLANT FACILITIES

Facilities
Acokk | Bunkaboeki | Horiuchi | Konan | Murakoshi
Murakoshi Industries | Nesstech | Nihon Flux | Nikkin Flux
NFK | Omega System | Organo | Taiyo Parker | Toyo Mic

Pump
Dynaflo | Ebara | Honda Kiko | KyowaMusashino
Tsurumi

Valve
Astam | Kyowa Iron | Nachi | Nippon Daiya | Sawada
Wasino Kiki | Yoshitake

Electricity
Arkon | Asahi Bagnal | Gentos | Iwasaki | Kokosha | U_RD

CONSTRUCTION

Concrete Work
Daia | EXEN | Japan Life | Mikasa | Okasan Kiko | Taiheiyo

Railway Work
Kyoei | Sanwa Tekki | Teikoku | Toko

Scaffolding
Bullman | Okabe | Rikiman | Tsugaru

High Tension Bolt
Dong Ah | KPF | Nippon Steel Bolten | Nippon Fastener

Bolt & Nut & Washer
Hard Lock | Kishu Fastener | Matsukin | Mori Kozai
Nakaumi | Naniwa | Ogawa | Otani | Sudo | Toneji

STEEL MATERIAL

Steel & other Material
Dongil | JIS Standard | DSR | Sumitomo Wire | Winoa IKK

Pipe
Benkan

Return Top