Main Characteristic Values
| Material | Density | Hardness (HRC) | Flexural Strength (GPa) | Tensile Strength (GPa) | Compressive Strength (0.2% offset) (GPa) | KIC (MPa·m1/2) | Young’s Modulus (GPa) | Poisson’s Ratio | Thermal Conductivity (W/m·K) | Coefficient of Thermal Expansion MK-1 (×10⁻⁶/°C) RT-673K (RT-400°C) | Coefficient of Thermal Expansion MK-1 (×10⁻⁶/°C) RT-873K (RT-600°C) |
|---|---|---|---|---|---|---|---|---|---|---|---|
| KF235ME (SKH57+VC) | 7.7 | 68 | 2.74 | 1.77 | 3.68 (3.33) | 31 | 215 | 0.24 | 18 | 9.0 | 9.7 |
| KF261ME (SKH57+VC, TiN) | 7.6 | 70 | 2.26 | 1.67 | 3.92 (3.83) | 19 | 220 | 0.24 | 19 | 9.4 | 9.9 |
| KF263ME (SKH57+VC, TiN) | 7.3 | 72 | 1.96 | 1.57 | 3.38 (3.33) | 13 | 230 | 0.23 | 20 | 8.8 | 9.4 |
| D40 | 14.55 | 74 | 3.50 | 2.30 | 5.1 (3.9) | 14 | 570 | 0.22 | 105 | 5.1 | 5.5 |
| U83 | 13.75 | 61 | 2.10 | 1.40 | 2.9 (-) | 53 | 510 | 0.23 | 112 | 6.2 | 6.7 |
| SKH51 | 8.1 | 64 | 3.92 | 1.91 | (2.75) | – | 217 | – | 27 | – | 10.8 |
| SKH57 | 8.2 | 65 | 2.06 | 1.86 | (2.84) | – | 230 | – | 25 | – | 11.8 |
| SKD11 | 7.7 | 61 | 3.43 | 2.26 | (2.26) | – | 206 | – | 29 | – | 12.9 |
| SKD61 | 7.8 | 54 | 2.75 | 2.16 | (1.96) | – | 206 | – | 31 | – | 13.8 |